What has to be controlled, and why

In an aluminium foundry the spectrometer is used for three different decisions, and each one stresses a different part of the element programme:

  • Melt correction before casting. Si, Mg, Cu, Zn, Fe, Mn, Ni, Cr, Ti and Zr decide whether the heat still matches the grade. A result that arrives after the mould is filled is only a record, not a correction.
  • Process control. Sodium, calcium or strontium for modification, and titanium or boron for grain refinement, are added in small amounts and fade with holding time. These elements need a method that can see them at the levels actually used.
  • Incoming and outgoing verification. Ingot certificates, returned scrap, and final cast certificates have to agree with the same calibration, otherwise the dispute lands on the foundry.

Iron and silicon are the two elements that most often decide whether a 6xxx heat is still inside the grade; in 7xxx the balance between zinc, magnesium and copper is what matters. A programme built for one family will not automatically serve the other, which is why the alloy list comes before the instrument model.

Why spark OES fits solid aluminium

Spark OES works on a solid, prepared sample. For aluminium that means a disc cut or cast from the melt, then surfaced on a lathe or mill so the analysis spot is clean and representative. Measurement is fast enough to sit inside the melting and holding cycle, and the full element programme is reported in one pass instead of one method per element.

The alternative methods each cover a narrower question: XRF is convenient for sorting and for silicon-heavy alloys but struggles with light elements and small concentrations; combustion analysis gives excellent carbon and sulfur but nothing else; wet chemistry is accurate and slow. In production, OES is the method that keeps the heat moving.

Configuration that matches the alloy list

Two platforms cover most aluminium work:

  • SDB-810 — 16-channel CCD, 130–700 nm. A practical choice when the alloy list is known and the element programme can be fixed around it.
  • SDB-910 — 16-channel CCD, 120–800 nm. The wider range is useful when the same laboratory also handles magnesium, nickel or copper bases, or when trace elements sit at the edge of the shorter wavelengths.

Both use an aluminium-base calibration with dedicated programmes for the families you cast. Ask for the calibration to be built against your grade list rather than a generic set: the difference shows up in the 0.1% range where most grade limits live. Argon quality, spark stand condition and sample preparation discipline matter as much as the channel count.

Sample form and workflow

A disc taken from the melt is the reference sample. It should be cast in a consistent mould, cooled under the same conditions, and surfaced identically every time — one lathe pass, no lubricant contamination, no overheated surface. For finished parts or ingot, a section cut from a representative area works, provided the cut avoids porosity and oxide skins.

  • Type-standardise at the start of the shift and after any maintenance.
  • Profile the grade before the heat is released, not after.
  • Keep a retained sample per heat so a later dispute can be re-checked on the same piece.
  • Record the instrument, programme and operator with each result.

For foundries that also cast other metals, the same bench can carry additional base programmes; the limit is sample preparation space and operator discipline, not the spectrometer itself.

What a useful quotation includes

A quotation that only names a model is not a configuration. The useful version states the base programmes, the element list per programme, the sample preparation equipment, the standards used for standardisation, the commissioning scope, and the training days. Send the alloy list, the sample form and the daily number of heats, and the configuration can be fixed before price.

Common questions

Can one OES cover both 6xxx and 7xxx?

Yes, provided the calibration includes both families and the element programme covers zinc, magnesium and copper at 7xxx levels. The risk is a programme built only around 6xxx and then stretched; ask for the grade list to be written into the calibration scope.

Is XRF enough for aluminium?

For sorting and rough grade checks it often is. For melt correction, modification and grain refiner control, the light elements and the small concentrations are where XRF becomes uncertain, and spark OES is the more reliable production method.

How often should the instrument be standardised?

At the start of each shift, after cleaning or maintenance, and whenever a control sample drifts outside its accepted window. The exact interval should follow your own quality procedure and the stability you actually observe.

Configure a system for this application

Send the alloy list, sample form and throughput